Home / Products / Spring Wire / Testing

Testing

Tensile and diameter per lot; relaxation data where the spring duty depends on it.

PropertyMethodEstablishesWhere
TensileASTM E8, per lotThe load the spring is designed fromCertificate
ElongationPer lotWhether the wire will coil without crackingCertificate
DiameterIn-line laser micrometer, 0.001 mmCoiling consistencyRecorded against the spool
SurfaceEddy current and visualDefects that become fatigue initiationReport
RelaxationStress relaxation testLoad retained at temperature and timeReport, on request

Why relaxation is a separate test

Tensile tells you the wire’s strength at room temperature; it does not tell you how much load the finished spring keeps after a thousand hours at 600 °C. Where that number matters, say so at enquiry and the relaxation test is scheduled rather than assumed.